Style Number | Temperature Rating | Voltage Rating | Dielectric Strength | Spark Test |
UL20689 | 90˚C | 150V | 2000V (AC/1min) | 3000V |
Construction Details
Conductor Material: TC – tinned copper.
Insulation: AWM verified material.
Shield: foil shield, braiding, copper strands wrapped, optional as per request.
Outer Jacket: quality polyurethane PUR.
Technical Parameters
//
Physical Properties
Aging Temperature: 113℃±2℃
Aging Period: 168HR
Tensile Strength after Aging: min 70%
Elongation after Aging: min 65%
Testing Temperature: 121℃±1℃
Testing Period: 1HR (60minutes)
Deformation: ≤50%
Testing Temperature: 121℃±1℃
Testing Period: 1HR (60minutes)
Heat Shock: No Crack
Testing Temperature: -10℃±2℃
Testing Period: 1HR (60minutes)
Cold Bend: No Crack
Reference Standard
UL Standard: UL758, UL
AWM Compliance: AWM
European Directive: EU Directive 2011/65/EU (RoHS 2), EU Directive 2012/19/EU (WEEE)
APAC Compliance: China RoHS II (GB/T 26572-2011)
Related products
-
UL20866
Read moreStyle Number Temperature Rating Voltage Rating Dielectric Strength Spark Test UL20866 80˚C 300V 2000V (AC/1min) 3000V Construction Details Conductor Material: TC – tinned copper. Insulation: AWM verified material. Shield: foil shield, braiding, copper strands wrapped, optional as per request. Outer Jacket: quality polyurethane PUR. Technical Parameters // Physical Properties Aging Temperature: 113℃±2℃ Aging Period: 168HR …
-
UL21029
Read moreStyle Number Temperature Rating Voltage Rating Dielectric Strength Spark Test UL21029 60/80˚C 600V 2000V (AC/1min) 3000V Construction Details Conductor Material: TC – tinned copper. Insulation: AWM verified material. Shield: foil shield, braiding, copper strands wrapped, optional as per request. Outer Jacket: quality polyurethane PUR. Technical Parameters // Physical Properties Aging Temperature: 113℃±2℃ Aging Period: 168HR …
-
UL20563
Read moreStyle Number Temperature Rating Voltage Rating Dielectric Strength Spark Test UL20563 60˚C 30V 2000V (AC/1min) 3000V Construction Details Conductor Material: TC – tinned copper. Insulation: AWM verified material. Shield: foil shield, braiding, copper strands wrapped, optional as per request. Outer Jacket: quality polyurethane PUR. Technical Parameters // Physical Properties Aging Temperature: 113℃±2℃ Aging Period: 168HR …
-
UL21127
Read moreStyle Number Temperature Rating Voltage Rating Dielectric Strength Spark Test UL21127 60/75˚C 600V 2000V (AC/1min) 3000V Construction Details Conductor Material: TC – tinned copper. Insulation: AWM verified material. Shield: foil shield, braiding, copper strands wrapped, optional as per request. Outer Jacket: quality polyurethane PUR. Technical Parameters // Physical Properties Aging Temperature: 113℃±2℃ Aging Period: 168HR …